  • Chemical composition of the abrasive material:

    SiO2 CaO Al2O3 MgO FeO
    30 ÷ 41 24,2 ÷ 26,2 11,5 ÷ 12,6 6,07 ÷ 10,4 4,6 ÷ 9,02
    K2O CuO ZnO Na2O PbO
    2,61 ÷ 3,9 0,9 ÷ 1,12 0,3 ÷ 0,88 0,4 ÷ 0,53 0,5 ÷ 1,00
    • Hardness: 6÷7 Mohsa

    • Content of free silica <1% -BIA No. 405222096

    • Proper electrical conductivity: maximally 25 mS/m

    • Content of chlorides soluble in water: 0.0025 % (m/m) max

    • Moisture content: maximally 0.20 %